| 钢的离子氮化表层中的α相微晶结构 |
| 李冀;苑永生;苑珂琦 |
| 东北工学院;东北工学院;教授;北京科技大学 |
|
| ALPHA-PHASE MICROCRYSTALLINE STRUCTURE OF IONITRIDING LAYER ON STEELS |
| LI Ji;YUAN Yongsheng Northeast University of Technology; Shenyang; YUAN Keqi University of Science and Technology Beijing |
引用本文:
李冀;苑永生;苑珂琦. 钢的离子氮化表层中的α相微晶结构[J]. 金属学报, 1991, 27(5): 148-150.
,
,
.
ALPHA-PHASE MICROCRYSTALLINE STRUCTURE OF IONITRIDING LAYER ON STEELS[J]. Acta Metall Sin, 1991, 27(5): 148-150.
1 Larsen B. Fφrland T. Mol Phys. 1973: 26: 1521 2 陈念贻,徐驰,李通化,江乃雄.中国科学(B辑),1987;(1) :21 3 徐驰,江乃雄,陈念贻.化学学报,1989:47:529 4 徐驰,陈念贻,江乃雄.物理化学学报,1987;3:55 5 Sangster M J L, Dixon M. Adv Phys, 1976; 25: 247 6 Holm J L, Kleppa O J. J Chem Phys, 1968; 49: 2425 7 Lumsden J. In: Inman D, Lovering D G eds., Ionic Liquids, New York: Plenum, 1981: 27--56 8 Fφrland T. J Phys Chem, 1955; 59: 152 9 Blander M. Molten Salt Chemistry, New York: Interscience, 1964: 127 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|