| 用柔度法和数值法确定疲劳裂纹的闭合效应 |
| 程育仁;施晓锋;彭湘;侯炳麟 |
| 北方交通大学;北方交通大学;北方交通大学;北方交通大学 |
|
| DETERMINATION OF FATIGUE CRACK CLOSURE EFFECT BY COMPLIANCE TECHNIQUE AND NUMERICAL METHOD |
| CHENG Yuren;SHI Xiaofeng;PENG Xiang;HOU Binglin Northern Jiaotong University; Beijing |
引用本文:
程育仁;施晓锋;彭湘;侯炳麟. 用柔度法和数值法确定疲劳裂纹的闭合效应[J]. 金属学报, 1991, 27(4): 43-48.
,
,
,
.
DETERMINATION OF FATIGUE CRACK CLOSURE EFFECT BY COMPLIANCE TECHNIQUE AND NUMERICAL METHOD[J]. Acta Metall Sin, 1991, 27(4): 43-48.