| Fe-Ni-Co-Ti合金中弥散析出的γ′粒子对马氏体形态的影响 |
| 崔立山;杨大智;李国斌;朱敏 |
| 锦州工学院;大连理工大学;大连理工大学;大连理工大学 |
|
| INFLUENCE OF DISPERSED γ′ ECIPITATEDPARTICLES ON MARTENSITE MORPHOLOGY IN Fe-Ni Co-Ti ALLOYS |
| CUI Lishan Jinzhou Institute of Technology; YANG Dazhi; LI Guobin ZHU Min Dalian University of Technology |
引用本文:
崔立山;杨大智;李国斌;朱敏. Fe-Ni-Co-Ti合金中弥散析出的γ′粒子对马氏体形态的影响[J]. 金属学报, 1991, 27(3): 46-50.
,
,
,
.
INFLUENCE OF DISPERSED γ′ ECIPITATEDPARTICLES ON MARTENSITE MORPHOLOGY IN Fe-Ni Co-Ti ALLOYS[J]. Acta Metall Sin, 1991, 27(3): 46-50.
1 Maki T, Kobayashi K, Minato M. Scr Metall, 1984; 18: 1105 2 Maki T, Kobayashi K, Tamura I. Proc Int Conf on Martensitic Transformations, (ICOMAT-82) , Leuven, Belgium, 1982: C4--541 3 Gunko L P, Koval Y N, Kozlova L Y, Kokorin V V, Osipenko I A. Phys Met Metall, 1982; 53(2) : 114, 118 4 Neuhauser H J, Pitsch W. Acta Metall, 1971; 19: 337 5 Patterson R L, Wayman C M. Acta Metall, 1964; 12: 1306; 1966; 14: 374 6 Reed R P. Acta Metall, 1967; 15: 1287 7 Maki T, Shimooka S. Umemoto M. Trans Jpn Inst Met, 1972; 13: 400 8 Fearon E O, Bevis M. Acta Metall. 1974; 22: 991 9 Miner R E. Metall Trans, 1971: 2: 1250 10 Maki T, Wayman C M. Acta Metall, 1977; 25: 695, 710 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|