| 晶粒间界局域无序化引起的滞弹性弛豫 |
| 程波林;葛庭燧 |
| 中国科学院固体物理研究所内耗与固体缺陷开放研究实验室;广州华南理工大学物理系;中国科学院固体物理研究所内耗与固体缺陷开放研究实验室;教授;合肥(230031) |
|
| ANELASTIC RELAXATIONS ASSOCIATED WITH LOCAL DISORDERING IN GRAIN BOUNDARIES |
| CHENG Bolin;GE Tingsui (T. S. Ke) (Laboratory of Internal Friction and Defects in Solids; Institute of Solid State Physics; Academia Sinica; Hefei |
引用本文:
程波林;葛庭燧. 晶粒间界局域无序化引起的滞弹性弛豫[J]. 金属学报, 1990, 26(5): 5-10.
,
.
ANELASTIC RELAXATIONS ASSOCIATED WITH LOCAL DISORDERING IN GRAIN BOUNDARIES[J]. Acta Metall Sin, 1990, 26(5): 5-10.
1 Kikuchi R, Cahn J W. Phys Rev, 1980; 21B: 1893 2 Kalonji G, Deymier P, Najafubadi R, Yip S. Surf Sci, 1984; 144: 77 3 Nguyen T, Yip S. Mater Sci Eng, 1989; 107: 15 4 Glicksman M E, Vold C L. Acta Metall, 1967; 15: 1409 5 Hsieh T E, Balluffi R W. Acta Metall, 1989; 37: 1637 6 Ke T S (葛庭燧). Ser Metall, 1990; 24: 347 7 Ke T S. (葛庭燧). Phys Rev, 1949; 76: 579 8 Seeger A, Weller M, Diehl J, Pan Zhengliang (潘正良), Zhang Jinxiu (张进修), Ke T S (葛庭燧).Z Metallk, 1982; 73: 1 9 Nowick A S, Berry B S. Anelastic Relaxation in Crystalline Solids, New York: Academic Press, 1972; 94 10 Ke T S (葛庭燧). J Appl Phys, 1949; 20: 274 11 Berger A, Wilbrandt P J, Haasen P. Acta Metall, 1983; 31: 1433 12 Fontaine C, Rocher A. J Microsc, 1980; 118: 105 13 Grabski M W. J Phys (Paris), Colloque, 1985; 46(C4) : 567 14 Watanabe T. J Phys (Paris), Colloque, 1985; 46(C4) : 555 15 Zhu A W (朱爱武), Ke T S (葛庭燧). Phys Status Solidi (a), 1989; 113: 393 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|