| 过冷液态金属热力学性质的变分计算 |
| 沈涛;王景唐 |
| 中国科学院金属研究所快速凝固非平衡合金实验室;中国科学院金属研究所快速凝固非平衡合金实验室;研究员;沈阳(110015) |
|
| VARIATIONAL CALCULATION OF THERMODYNAMIC PROPERTIES OF SUPERCOOLED LIQUID METALS |
| SHEN Tao; WANG Jingtang Institute of Metal Research Academia Sinica; Laboratory of Rapidly Solidified Non-Equilibrium Alloys; Shenyang professor |
引用本文:
沈涛;王景唐. 过冷液态金属热力学性质的变分计算[J]. 金属学报, 1990, 26(3): 119-125.
,
.
VARIATIONAL CALCULATION OF THERMODYNAMIC PROPERTIES OF SUPERCOOLED LIQUID METALS[J]. Acta Metall Sin, 1990, 26(3): 119-125.
1 Klinger M I. Phys Rep, 1988; 165: 275 2 Jaeckle J. Rep Prog Phys, 1986; 49: 171 3 Shimoji M. Liquid Metals, New York: Academic Press, 1977 4 Heine V. Solid State Phys, 1970; 24: 1 5 Li D H, Li X R, Wang S. J Phys, 1986; F16: 309 6 Woo C H, Wang S, Matsuura M. J Phys, 1975; F5: 1836 7 Li D H, Moore R A, Wang S. Can J Phys, 1986; 64: 75 Li D H, Moore R A, Wang S. Can J Phys, 1986; 64: 852 8 Li D H, Moore R A, Wang S. J Chem Phys, 1988; 88: 2700 Li D H, Moore R A, Wang S. J Chem Phys, 1988; 89: 4309 9 Ashcroft N W, Lekner J. Phys Rev, 1966; 145: 83 10 Hultgren R, Desai P D, Hawkins D T, Gleiser M, Kelley K K, Wagman D D. Selected Values of the Thermodynamic Properties of the Elements, Ohio: ASM, 1973 11 Brandes E A. Smithells Metals Reference Book. 6th ed, London: Butterworth, 1983 12 Cohen M H, Grest G S. Phys Rev, 1979; B20: 1077| |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|