| M_1-M_2-x-y系优势区相图的绘制及其应用 |
| 王龙章;黄克雄;骆如铁;姚渝;叶大陆;陈新民 |
| 中南工业大学化学系;工程师;长沙(410083);中南工业大学;中南工业大学;中南工业大学;中南工业大学;中南工业大学 |
|
| DRAWING PREDOMINANCE DIAGRAM OF M_1-M_2-x-y SYSTEM AND ITS APPLICATION |
| WANG Longzhang;HUANG Kexiong;LUO Rutie;YAO Yu;YE Dalu;CHEN Xinmin Central South University of Technology; Changsha Department of Chemistry;Central South University of Technology;Changsha 410083 |
引用本文:
王龙章;黄克雄;骆如铁;姚渝;叶大陆;陈新民. M_1-M_2-x-y系优势区相图的绘制及其应用[J]. 金属学报, 1990, 26(3): 113-118.
,
,
,
,
,
.
DRAWING PREDOMINANCE DIAGRAM OF M_1-M_2-x-y SYSTEM AND ITS APPLICATION[J]. Acta Metall Sin, 1990, 26(3): 113-118.
1 Sohn Hongyong. Miner Sci Eng, 1979; 11 (3) : 24 2 Turkdogan E T. Physical Chemistry of High Temperature Technology, New York: Academic Press, 1980 3 王龙章,陈新民.中南矿冶学院学报,待发表 4 东北工学院有色重金属冶炼教研室等.锌冶金,北京:冶金工业出版社,1978:15+ |
|