| 一种新的钼氧化物相 |
| 方正;张平民;陈新民 |
| 中南工业大学化学系;副教授;长沙(410083);中南工业大学;中南工业大学 |
|
| A NEW MOLYBDENUM OXIDE PHASE |
| FANG Zheng;ZHANG Pingmin;CHEN Xinmin Central South University of Technology; Changsha associate professor;Department of Chemistry;Central South University of Technology; Changsha 410083 |
引用本文:
方正;张平民;陈新民. 一种新的钼氧化物相[J]. 金属学报, 1990, 26(2): 98-101.
,
,
.
A NEW MOLYBDENUM OXIDE PHASE[J]. Acta Metall Sin, 1990, 26(2): 98-101.
1 Werner P E, Eriksson L. Westdahl M. J Appl Crystallogr, 1985; 18: 367 2 Kihlborg L, Magneli A. Acta Chem Scand, 1955; 9: 471 3 Yoda E. J Phys Soc Jpn, 1960; 15: 821 4 JCPDS. Powder Diffraction File, sets 21--22, 1980: 183 5 Staskiewicz B A, Tucker J R, Snyder P E. J Am Chem Soc, 1955; 77: 2987 6 Mah A D. J Phys Chem, 1957; 61 (11) : 1572 7 Hagg G, Magneli A. Ark Kemi Mineral Geol, 1945; A19: 1 8 #12 9 Brewer L. Chem Rev. 1953; 52: 1 |
|