| 恒氧位下渣-熔Cu间Ti和Si的传输 |
| 薛向欣;杜鹤桂 |
| 东北工学院;313信箱沈阳(110006);东北工学院 |
|
| TRANSFER OF Ti AND Si BETWEEN SLAGS AND MOLTEN Cu UNDER CONSTANT OXYGEN POTENTIAL |
| XUE Xiangxin;DU Hegui Northeast University of Technology; Shenyang Department of Ferrous Metallurgy;Northeast University of Technology; Shenyang 110006 |
引用本文:
薛向欣;杜鹤桂. 恒氧位下渣-熔Cu间Ti和Si的传输[J]. 金属学报, 1990, 26(2): 146-148.
,
.
TRANSFER OF Ti AND Si BETWEEN SLAGS AND MOLTEN Cu UNDER CONSTANT OXYGEN POTENTIAL[J]. Acta Metall Sin, 1990, 26(2): 146-148.
1 Baxter G P, Lansing J E. J Amer Chem Soc, 1920; 42: 419 2 周继程,邹元爔,赵彭年,李鸿明,张子青.中国金属学会编,中国金属学会1979--1980年优秀论文集,第四分册,北京:冶金工业出版社,1984:83 3 森一美,平沢政(广厶),新贝元,圃中朝夫.铁钢,1985;71:1110 4 薛向欣,杜鹤桂.金属学报,1990;26:B7 |
|