| 含H_2O气氛下Cu液中Ti的氧化 |
| 薛向欣;杜鹤桂 |
| 东北工学院;313信箱沈阳(110006);东北工学院 |
|
| OXIDATION OF Ti IN MOLTEN Cu UNDER WATERY ATMOSPHERE |
| XUE Xiangxin;DU Hegui Northeast University of Technology; Shenyang Department of Ferrous Metallurgy;Northeast University of Technology;Shenyang;110006 |
引用本文:
薛向欣;杜鹤桂. 含H_2O气氛下Cu液中Ti的氧化[J]. 金属学报, 1990, 26(1): 153-154.
,
.
OXIDATION OF Ti IN MOLTEN Cu UNDER WATERY ATMOSPHERE[J]. Acta Metall Sin, 1990, 26(1): 153-154.
1 周继程,邹元(忄羲),赵彭年,李鸿明,张子青.见:中国金属学会编,中国金属学会1979--1980年优秀论文集,第四分册,北京:冶金工业出版社,1984:83 2 Wagner C. Z Phy Chem, 1933; B21: 25 3 Edstrom J O, Bitsianes G. J Met, 1955; 7: 760 4 中井弘.铁钢,1961;47:161 |
|