| 铸态耐磨锰钢碳化物的团球化 |
| 姜启川;何镇明;阎久林;崔东焕;王守实 |
| 吉林工业大学铸造教研究;副教授;长春(130025);吉林工业大学;吉林工业大学;吉林工业大学;吉林工业大学 |
|
| NODULARIZATION OF CARBIDE IN AS-CAST WEAR-RESISTANT MANGANESE STEEL |
| JIANG Qichuan;HE Zhenming;YAN Jiulin;CUI Donghuan;WANG Shoushi Jilin University of Technology; Changchun Associate Professor;Faculty of Cast; Jilin University of Technology; Changchun 130025 |
引用本文:
姜启川;何镇明;阎久林;崔东焕;王守实. 铸态耐磨锰钢碳化物的团球化[J]. 金属学报, 1990, 26(1): 151-152.
,
,
,
,
.
NODULARIZATION OF CARBIDE IN AS-CAST WEAR-RESISTANT MANGANESE STEEL[J]. Acta Metall Sin, 1990, 26(1): 151-152.
|