| Fe-Cr-Mn奥氏体合金的辐照体胀与诱起晶界偏析行为的研究 |
| 胡本芙;高桥平七郎;伊藤久敏;竹山太郎 |
| 北京科技大学材料科学及工程系金相教研组;副教授;北京(100083);日本北海道大学;日本北海道大学;日本北海道大学 |
|
| BEHAVIOR OF VOID SWELLING AND RADIATION-INDUCED SEGREGATION IN Fe-Cr-Mn ALLOY SYSTEM UNDER ELECTRON IRRADIATION |
| HU Benfu;TAKAHASHI Heishichiro;ITOH Hisatoshi;TAKEYAMA Taro University of Science and Technology Beijing Hokkaido University; Sapporo; Japan Section of Metallography; Department of Materials;University of Science and Technology Beijing; Beijing 100083 |
引用本文:
胡本芙;高桥平七郎;伊藤久敏;竹山太郎. Fe-Cr-Mn奥氏体合金的辐照体胀与诱起晶界偏析行为的研究[J]. 金属学报, 1990, 26(1): 1-7.
,
,
,
.
BEHAVIOR OF VOID SWELLING AND RADIATION-INDUCED SEGREGATION IN Fe-Cr-Mn ALLOY SYSTEM UNDER ELECTRON IRRADIATION[J]. Acta Metall Sin, 1990, 26(1): 1-7.
1 Harries D R, Proceedings, Topical Conference on Ferritic Alloys for Use in Nuclear Energy Technologies, Americall Intstitute of Minging Metallurgical and Petroleum Engineers, 1983: 141--155 2 Bott A H, Pickering F B, Butterworth G J. J Nucl Mater, 1986; 141--143: 1088--1096 3 Franks R, Binder W O, Thompson J. Trans ASM, 1955; 47: 231--266 4 Taleyama T, Takahashi H, Ohnuki S. J Nucl Mater, 1982; 108&109: 465 5 Brager H R, Garner F A, Gelles D S, Hamilton M L. J Nucl Mater, 1985; 133&134: 907--911 6 Hu Benfu(胡本芙), Takahashi H, Proceeding of the 2th China-Japan Metal Physics and Physical Metallurgy Symposium, Kunming, 1986: 151 7 石野?,照射损伤,东京大学出版社,1979:16--21 8 胡本芙,高桥平六郎,竹山太郎.金属学报,1988;24:A180 9 Oikawa H. Tech Rep Tohoku Unive, 1982; 47: 215 10 Anthony T R. In: Corbett J W, Ianniello L C eds., Radiation-Induced Voids in Metals, Springfield, V A: Nat Tech Infor-Mation Service, 1972: 63 |
|