| Al-Si共晶强制性非稳态生长实验研究 |
| 刘俊明;周尧和;商宝禄 |
| 西北工业大学;西北工业大学;西北工业大学 |
|
| NONSTABLE GROWTH OF Al-Si EUTECTIC IN CONSTRAINED CONDITION |
| LIU Junming;ZHOU Yaohe;SHANG Baolu Northwestern Polytechnical University; Xi'an |
引用本文:
刘俊明;周尧和;商宝禄. Al-Si共晶强制性非稳态生长实验研究[J]. 金属学报, 1989, 25(6): 102-107.
,
,
.
NONSTABLE GROWTH OF Al-Si EUTECTIC IN CONSTRAINED CONDITION[J]. Acta Metall Sin, 1989, 25(6): 102-107.
1 Jackson K A, Hunt J D. TMS AIME, 1966; 236: 1129 2 Cline H E. TMS AIME, 1969; 245: 2205 3 Jordan R M, Hunt J D. Metall Trans, 1971; 2: 3401 4 Elliott R. Eutectic Solidification Processing, Crystalline and Glassy Alloys, London: Butterworths, 1983 5 Zener C. TMS AIME, 1946; 167: 550 6 Elliott R. Glenister S M D. Acta Metall, 1980; 28: 1489 7 Hogan L Mi Song H. Metall Trans, 1987; 18A: 707 8 Carlberg T, Fredrirsson H. J Cryst Growth, 1977; 42: 526 9 刘俊明,周尧和,商宝禄.西北工业大学学报,1989;7(4) :601; |
|