氧对H_2O-H_2及H_2O-H_2惰气混合气体氧位的影响
方正;陈新民
中南工业大学;中南工业大学
EFFECT OF OXYGEN CONTENTS ON OXYGEN POTENTIALS OF H_2O-H_2 AND H_2O-H_2-INERTS GAS MIXTURES
FANG Zheng;CHEN Xinmin H. M Chen Central South University of Technology; Changsha
引用本文:

方正;陈新民. 氧对H_2O-H_2及H_2O-H_2惰气混合气体氧位的影响[J]. 金属学报, 1989, 25(4): 81-88.
, . EFFECT OF OXYGEN CONTENTS ON OXYGEN POTENTIALS OF H_2O-H_2 AND H_2O-H_2-INERTS GAS MIXTURES[J]. Acta Metall Sin, 1989, 25(4): 81-88.

全文: PDF(624 KB)  
摘要: 考虑到氧的影响,本文导出一组H_2O-H_2及H_2O-H_2-惰气混合气体氧位新的表征式。经典表征式是该公式的特例。本文讨论了微量氧存在时对平衡气氛影响的各种因素以及减小误差的最佳配气条件,同时评价了某些用H_2O-H_2(或H_2O-H_2-惰气)混合气体控制氧位的平衡实验的可靠程度。
关键词 : 气体平衡法,  H_2O-H_2,  H_2O-H_2-惰气,  氧位    
Abstract:By taking the effect of oxygen contents into account, a new set offormulae which represents the oxygen potentials of H_2O-H_2 and H_2O-H_2-inerts gasmixtures has been derived. Classical representation is only a particular case of it.Some of the variables affecting the equilibrium atmosphere when trace oxygen ispresent and optimum preparation of the gas mixtures to minimize errors have beendiscussed. The reliability of some of previous equilibrium experiments under theoxygen potentials controlled by H_2O-H_2 or H_2O-H_2-inerts gas mixtures has alsobeen criticized.
Key words: gas equilibration method    H_2O-H_2    H_2O-H_2-inerts    oxygen potential
收稿日期: 1989-04-18     
基金资助:国家自然科学基金
1 Emmett P H, Shultz J F. J Am Chem Soc, 1929; 51: 3249
2 Shibata Z, Kitagawa H. J Fac Sci, 1938; 2: 223
3 Muan A. Am J Sci, 1958; 256 (3) : 171
4 Pierre G R St., Ebihara W T, Pool M J, Speiser R. Trans AIME, 1962; 224: 259
5 Rapp R A. Physicochemical Measurements in Metals Research, Vol. Ⅳ, New York: Interscience, 1970: 338
6 Gaskell D R. Introduction to Metallurgical Thermodynamics. 2nd Ed., New York: Hemisphere Publishing, 1981: 242
7 王常珍.冶金物理化学研究方法,北京:冶金工业出版社,1982:230
8 方正,陈新民.中南矿冶学院学报,1982;13(4) :1
9 方正,陈新民.金属学报,1988;24:B41
10 方正,陈新民.第七届冶金过程物理化学年会和第二届有色冶金物理化学年会论文集,中国金属学会,中国有色金属学会,沈阳,1989:59
11 Sardi A. Acta Chim Hung, 1963; 38: 177
[1] 陈二保; 董元篪; 郭上型 . Mn-Fe熔体的脱Si过程及Mn-Fe熔体氧位研究[J]. 金属学报, 2001, 37(4): 400-404 .
[2] 方正;陈新民. 非化学计量Mo与MoO_2的平衡——兼论Sieverts常数在Smiltens积分中的应用[J]. 金属学报, 1988, 24(1): 111-113.