电化学合金化Y-Cu体系的生成自由能
杨绮琴;刘冠昆;刘泽锦
中山大学;中山大学;中山大学
FREE ENERGIES OF FORMATION FOR ELECTROCHEMICALLY ALLOYED Y-Cu SYSTEM
YANG Qiqin;LIU Cuankun;LIU Zejin Zhongshan University; Guangzhou
引用本文:

杨绮琴;刘冠昆;刘泽锦. 电化学合金化Y-Cu体系的生成自由能[J]. 金属学报, 1989, 25(4): 110-114.
, , . FREE ENERGIES OF FORMATION FOR ELECTROCHEMICALLY ALLOYED Y-Cu SYSTEM[J]. Acta Metall Sin, 1989, 25(4): 110-114.

全文: PDF(401 KB)  
摘要: 本文研究了在NaCl-KCl-YCl_3熔体中,电化学合金化Y-Cu体系的热力学行为。用恒电位电解断电后的电极电位-时间曲线测定了形成YCu_6,YCu_4,YCu_2,YCu等金属间化合物反应的ΔG(973-1103K),结果表明测量方法简单可靠。
关键词 : 钇—铜合金,  生成自由能,  电化学合金化    
Abstract:The electrochemical alloying of Y-Cu system in molten NaCl-KCl-YCl_3 has been investigated. The free energy changes of the formation reactions ofthe intermetallic compounds, including YCu_6, YCu_4, YCu_2, YCu(973--1103K), weredetermined by means of electrode potential-time curves of the working electrodeafter potentiostatic electrolysis. The results indicate that the potential-time methodis simple and reliable.
Key words: Y-Cu system    free energy of formation    electrochemically alloying
收稿日期: 1989-04-18     
基金资助:国家自然科学基金
1 Lesourd J-B P F, Plambeck J A. Can J Chem, 1969; 47: 3387
2 #12
3 #12
4 Wen C J. Boukamp B A. Huggins R A, Weppner W. J Electrochem Soc, 1979; 126: 2258
5 Picard G S. Mottot Y E, Tremillon B L. Proc 4th Int. Molten Salt Symp. Eds. Blander M, Newman D S, Saboungi M L, Mamantov G. Johnson K 84--2, 585 (1984) . The Electrochemical Society Inc., Pennington, N. J.
6 乔芝郁,Taxi P.金属学报,1987;23:B76
7 #12
8 Flengas S N. Ingraham T R. J Electrochem Soc. 1959; 106: 714
9 #12
10 章复中,谷力军.稀土,1983;(3) :67
[1] 李文超;王俭;李兴康;刘四俊;孙贵如. 金属间化合物的热力学数据及其稳定性判定[J]. 金属学报, 1994, 30(15): 97-103.
[2] 杨绮琴;刘冠昆;童叶翔;梁广超. Ni在NaCl-KCl-PrCl_3熔体中的电化学合金化[J]. 金属学报, 1992, 28(3): 65-68.
[3] 郑敏辉;陈一松. 电动势法测定Na_2SnO_3的生成自由能[J]. 金属学报, 1992, 28(2): 91-93.