| NaCl-BaCl_2-SrCl_2三元熔盐相图的计算 |
| 李瑞青;周国治 |
| 北京有色金属研究总院;北京科技大学 |
|
| CALCULATION OF NaCl-BaCl_2-SrCl_2 PHASE DIAGRAM |
| LI Ruiqing;ZHOU Guozhi Beijing General Research Institute for Non-Ferrous Metals University of Science and Technology Beijing |
引用本文:
李瑞青;周国治. NaCl-BaCl_2-SrCl_2三元熔盐相图的计算[J]. 金属学报, 1989, 25(3): 90-95.
,
.
CALCULATION OF NaCl-BaCl_2-SrCl_2 PHASE DIAGRAM[J]. Acta Metall Sin, 1989, 25(3): 90-95.
1 Levin E M, Robbins C R, Mcmurdie H F. In: Reser M K ed, Phase Diagrams for Ceramists. and 1969, 1975 Suppl., Columbus, Ohio: American Ceramic Society, Fig. 1428 2 周国治,李瑞青.稀有金属,待发表 3 Barin I, Knacke O, Kubaschewski O. Thermochemical Properties of Inorganic Substances, Springer-Verlag, Berlin, 1977 4 Levin E M, Robbins C R, Mcmurdie H F. In: Reser M K ed, Phase Diagrams for Ceramists, and 1969, 1975 Suppl., Columbus, Ohio: American Ceramic Society, Fig. 1311 5 Emons H H, Brautigan G, Thomas R. Chem Zvesti, 1978; 32 (6) : 721 6 1968; 13 (8) ; 2251 7 Levin E M, Robbins C R, Mcmurdie H F. In: Reser M K ed, Phase Diagrams for Ceramists, and 1969, 1975 Suppl., Columbus. Ohio: American Ceramic Society, Fig. 1301 8 Egan J J. Bracker J. J Chem Thermodyn, 1974; 6: 9 9 Qiao Zhiyu (乔芝郁), James Sangster. Pelton A D. CALPHAD, 1987; 11: 10 Papatheodorou G N. Kleppa O J. J Chem Phys, 1967; 47: 2014 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|