| 制备条件对非晶态Fe_(78)B_(13)Si_9合金的热膨胀各向异性的影响 |
| 陆坚;王景唐;丁炳哲 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| EFFECT OF PREPARATION CONDITION ON THERMAL EXPANSION ANISOTROPY FOR AMORPHOUS Fe_(78)B_(13)Si_9 ALLOY |
| LU Jian;WANG Jingtang;DING Bingzhe Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
陆坚;王景唐;丁炳哲. 制备条件对非晶态Fe_(78)B_(13)Si_9合金的热膨胀各向异性的影响[J]. 金属学报, 1989, 25(3): 102-106.
,
,
.
EFFECT OF PREPARATION CONDITION ON THERMAL EXPANSION ANISOTROPY FOR AMORPHOUS Fe_(78)B_(13)Si_9 ALLOY[J]. Acta Metall Sin, 1989, 25(3): 102-106.
1 Kraus L, Tomas I, Kratochvilova E, Springmann B, Muller E. Phys Status Solidi (a), 1987; 100: 289 2 Zaveta K, Schneider J, Springmann B. Czech J Phys, 1985: B35: 289 3 Luborsky F E, Becker J J, McCary R O. IEEE Trans Magn, 1975; MAG11: 1644 4 Fujimori H. Obi Y, Masumoto T, Saito H. Mater Sci Eng, 1976; 23: 281 5 Morita H, Fujimori H, Obi Y. Appl Phys, 1979; 20: 125 6 E du Tremolet de Lacheisserie. J Magn Magn Mater, 1987; 66: 102 7 Arakawa S, Harada H, Hausch G. Hilziuger H R, Menges F J, Warlimont H. In: Steeb S ed, Rapidly Quenched Metals, Vol. Ⅱ, Proc 5th Int Conf on Rapidly Quenched Metals, at Germany Sept., 3--7, 1984. North-Holland, 1985: 1389 8 Pang Dexing (庞德兴), Wang Jingtang (王景唐), Song Qihong (宋启洪), et al. J Phys D: Appl Phys, 1987; 20: 1544 9 Wang Jingtang (王景唐), Ding Bingzhe (丁炳哲), Li Shuling (李淑苓), Wei Xueli (隗学礼). In: Steeb S ed, Rapidly Quenched Metals, Vol. Ⅱ, Proc 5th Int Conf on Rapidly Quenched Metals, at Germany Sept., 3--7, 1984, North--Holland, 1985: 1361 10 Toeroek E. Hausch G, J Magn Magn Mater, 1979; 10: 303 |
|