| 用最大熵方法从Ni-P非晶态合金X射线数据求径向分布函数 |
| 梁健端;林树智 |
| 中国科学院金属研究所;长沙国防科技大学;中国科学院金属研究所;副研究员;沈阳 |
|
| APPLICATION OF MAXIMUM ENTROPY METHOD TO CALCULATE RDF OF Ni-P AMORPHOUS ALLOY FROM X-RAY DIFFRACTION DATA |
| LIANG Jianduan;LIN Shuzhi Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
梁健端;林树智. 用最大熵方法从Ni-P非晶态合金X射线数据求径向分布函数[J]. 金属学报, 1989, 25(1): 141-146.
,
.
APPLICATION OF MAXIMUM ENTROPY METHOD TO CALCULATE RDF OF Ni-P AMORPHOUS ALLOY FROM X-RAY DIFFRACTION DATA[J]. Acta Metall Sin, 1989, 25(1): 141-146.