超塑变形的特征参数
崔建忠;马龙翔
东北工学院;317信箱讲师;东北工学院
CHARACTERISTIC PARAMETERS IN SUPERPLASTIC DEFORMATION
CUI Jianzhong;MA Longxiang Northeast University of Technology; ShenyangCUI Jianzhong Lecturer;P.O.Box 317;Northpast Uninersity of Technology;Shenyang
引用本文:

崔建忠;马龙翔. 超塑变形的特征参数[J]. 金属学报, 1988, 24(1): 92-96.
, . CHARACTERISTIC PARAMETERS IN SUPERPLASTIC DEFORMATION[J]. Acta Metall Sin, 1988, 24(1): 92-96.

全文: PDF(345 KB)  
摘要: 本文确定了超塑变形多重机制效应的存在,并根据这个效应,分析了超塑变形的主要参数,m,P和Q_a的变化规律及产生这些变化的原因.
关键词 超塑变形应变速率敏感性指数m值晶粒尺寸指数P激活能Q_α    
Abstract:The change of the characteristic parameters, strain rate sensiti-vity m, activation energy Q_a and grain size exponent P with changing strain rateand temperature and their physical reason have be n analysed according to the mul-tiple machanism effect in superplastic deformation. Their quantitative expressionshave also been given.
Key wordssuperplastic deformation    strain rate sensitivity    grain size exponent    activation energy
收稿日期: 1988-01-18     
1 崔建忠.装甲铝合金超塑性研究,东北工学院博士论文,1985
2 松木贤司,针山典笃,时沢贡,日本金属学会志,1981;45:935
3 Weertman J. J Appl Phys, 1955; 26: 1213
4 Herring C H. J Appl Phys, 1950; 21: 437
5 Edington J W. Melton K N, Cutler C P. Prog Mater Sci, 1975--1976; 21: 616
[1] 刘志义; 刘冰 . 脉冲电流对2091Al-Li合金超塑变形机理的影响[J]. 金属学报, 2000, 36(9): 944-951 .
[2] 颜莹; 张彩碚; 刘渤然 . 铝合金及其复合材料在超塑变形过程中的正电子寿命谱[J]. 金属学报, 1999, 35(12): 1284-1288 .
[3] 李淼泉;吴诗惇. LY12CZ铝合金超塑变形时的电场效应[J]. 金属学报, 1995, 31(6): 272-276.
[4] 刘庆;杨王玥;陈国良;吴以琴. Ti-12Co-5Al合金的超塑变形[J]. 金属学报, 1994, 30(17): 223-228.
[5] 刘庆;刘振纲;姚枚. 温轧态Al-Li-Cu-Mg-Zr合金超塑变形后空洞行为与残余强度的研究[J]. 金属学报, 1993, 29(9): 25-30.
[6] 刘庆;黄晓旭;姚枚;杨金凤. 拉伸条件对Al-Li-Cu-Mg-Zr合金超塑变形行为的影响[J]. 金属学报, 1991, 27(6): 126-132.
[7] 蒋兴钢;崔建忠;马龙翔. 高强度7475Al合金超塑变形空洞形状变化的分形描述[J]. 金属学报, 1990, 26(4): 144-147.
[8] 崔建忠;马龙翔. 超塑变形中的晶粒形状效应[J]. 金属学报, 1988, 24(4): 354-361.