| Ce和Nd在α-Fe中的固溶度 |
| 章复中;谷力军;瞿柳兴;刘沃垣;颜玉新 |
| 包头稀土研究院;包头稀土研究院;包头稀土研究院;包头稀土研究院;包头稀土研究院 |
|
| SOLID SOLUBILITIES OF Ce AND Nd IN α-Fe |
| by ZHANG Fuzhong; GU Lijun; OU Liuxing; LIU Woyuan; YAN Yuxin (Baotou Rare Earth Research Institute) (Manuscript received 25 September; 1986) |
引用本文:
章复中;谷力军;瞿柳兴;刘沃垣;颜玉新. Ce和Nd在α-Fe中的固溶度[J]. 金属学报, 1987, 23(6): 503-506.
,
,
,
,
.
SOLID SOLUBILITIES OF Ce AND Nd IN α-Fe[J]. Acta Metall Sin, 1987, 23(6): 503-506.
1 Jepson J O, Duwez P. Trans ASM, 1955; 47: 543-553 2 Richerd J. Mem Sci Roy Metall, 1962; 59: 527 3 Haefling J F, Daane AH. In: Spedding F H, Daane A H eds., The Rare Earth, New York: Wiley, 1961: 280 4 #12 5 庄应烘,荣国器,唐晓峰.中国稀土学报,1983;1(1) :58-61 6 #12 7 Domagala R F, Rausch J J, Levinson D W. Trans ASM, 1961; 53: 137-155 8 颜玉新,章复中.稀有金属(季刊),1987;6(2) :131 9 #12 |
|