| 快速凝固钼合金的显微结构与时效硬化 |
| 宁远涛;S.H.Whang |
| 昆明贵金属研究所;BarnettInstituteofNortheasternUniversity;Boston;USA |
|
| MICROSTRUCTURE AND AGE HARDENING IN RAPIDLY SOLIDIFIED Mo ALLOYS |
| by NING Yuantao (Institute of Precious Metals; Kunming); WHANG; S. H. (Barnett Institute of Northeastern University; Boston; USA) (Manuscript received 27 August; 1986; revised manuscript 11 March; 1987) |
引用本文:
宁远涛;S.H.Whang. 快速凝固钼合金的显微结构与时效硬化[J]. 金属学报, 1987, 23(6): 491-497.
,
.
MICROSTRUCTURE AND AGE HARDENING IN RAPIDLY SOLIDIFIED Mo ALLOYS[J]. Acta Metall Sin, 1987, 23(6): 491-497.
1 Whang S H, Giessen B C. PROC 3rd Conf Rapid Solidification Processing, Washington D C: NBS, 1982: 439 2 Whang S H. J Met, 1984; 36(4) : 34 3 Moffatt WG. Binary Phase Diagram Handbook, Vol.Ⅰ, B-Mo Phase Diagram, General Electric Company, Printed in USA, 1976 4 Moffatt W G. Binary Phase Diagram Handbook, Vol. Ⅰ, B-Er Phase Diagram, General, Electric Company, Printed in USA, 1976 5 Selected Powder Diffraction Data, Metal and Alloys Data Book, First Edition, Published by the International Centre for Diffraction Data, Ⅱ, 25-561, 1978: 616 6 Shunk F A. Constitution of Binary Alloys, Second Supplement, New York: McGraw-Hill, 1969: 91 7 Selected Powder Diffractopm Data, Metal and Alloys Data Book, First Edition, Published by the International Centre for Diffraction Data, Ⅰ, 6-610, 1978: 156 8 Elliott R P. Constitution of Binary Alloys, First Supplement, New York: McGraw-Hill, 1965: 1464 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|