Ce对低硫16Mn钢凝固组织的影响 |
胡汉起;钟雪友;韩青有 |
北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
EFFECT OF Ce ON SOLIDIFICATION STRUCTURE OF LOW SULPHUR 16 Mn STEEL |
HU Hanqi; ZHONG Xueyou; HAN Qingyou (Beijing University of Iron and Steel Technology) (Manuscript received 21 November; 1984; revised manuscript 7 November; 1985) |
引用本文:
胡汉起;钟雪友;韩青有. Ce对低硫16Mn钢凝固组织的影响[J]. 金属学报, 1987, 23(3): 176-181.
,
,
.
EFFECT OF Ce ON SOLIDIFICATION STRUCTURE OF LOW SULPHUR 16 Mn STEEL[J]. Acta Metall Sin, 1987, 23(3): 176-181.
1 钟雪友,胡汉起,刘昌明.北京钢铁学院学报,1984;(3) :16 2 Flenings M C. Solidification Processing, New York: McGraw-Hill, 1974:42 3 Jacobi H, Schwerdtfeger K. Metall Trans. 1976; 7A: 811 4 塗嘉夫,大橋徹郎,広本键,北村修.鉄鋼,1980;62:614 5 胡汉起,钟雪友,力航.金属学报,1984;20:A247 6 胡汉起,钟雪友,力航.北京钢铁学院学报,1983;(1) :64 7 韩青有,胡汉起.北京钢铁学院学报,1985;(1) :1 |
|