| 双相钢微观变形行为的动态研究 |
| 沈显璞;雷廷权;刘剑壮 |
| 冶金工业部钢铁研究总院;哈尔滨工业大学;哈尔滨工业大学 |
|
| A DYNAMIC OBSERVATION OF MICROSCOPIC DEFORMATION BEHAVIOR IN DUAL-PHASE STEELS |
| SHEN Xianpu (Central Tron and Steel Research Institute; Ministry oj Metallurgical Industry; Beijing); LEI Tingquan; LIU Jianzhuang (Harbin Institute of Technology) (Manuscript received 21 May; 1985; revised manuscript 28 April; 1986) |
引用本文:
沈显璞;雷廷权;刘剑壮. 双相钢微观变形行为的动态研究[J]. 金属学报, 1987, 23(2): 150-245.
,
,
.
A DYNAMIC OBSERVATION OF MICROSCOPIC DEFORMATION BEHAVIOR IN DUAL-PHASE STEELS[J]. Acta Metall Sin, 1987, 23(2): 150-245.
1 沈显璞,雷廷权.金属学报,1985;21:A228 2 沈显璞,雷廷权.金属学报,1984;20:A266 3 Shen H P (沈显璞),Lei T C(雷廷权).Met Sci 1984; 19: 275 4 田村今男,友田陽,山岡幸男,金谷三郎,小沢正俊,赤尾明,鉄鋼,1973;59:454 5 Davies R G. Metall Trans 1978; 9A: 451 6 Araki K, Takada Y, Nakaoka K. Trans Ionr Steel Inst Jpn 1977; 17:710 7 Tomota Y, Kuroki K, Mori t, Tamura I. Mater Sci Eng 1976; 24: 85 8 雷廷权,沈显璞,金属学报,1982;18:75 9 Lei TC(雷廷权),Shen HP(沈显璞). In: MC Queen H J, Bailon J-P, et al eds Strength of Metals and Alloys. New York: Oxford, Pergamon Press, 1985, Vol. 2: 1007 10 Davies R G. Metall Trans 1978; 9A: 691 11 Wan C M, Yie S N,Jahn M T,Kuo S M.J Meatr Sci 1981; 16: 2682 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|