ACTIVITY OF As IN Fe-As-C-j MELTS
by DONG Yuanchi; WEI Shoukun;PENG Yuqiang; ZHU Yuankai (Beijing University of Iron and Steel Technology)
引用本文:

董元篪;魏寿昆;彭(忄育)强;朱元凯. Fe-As-C-j熔体中As活度的研究[J]. 金属学报, 1986, 22(6): 89-91.
, , , . ACTIVITY OF As IN Fe-As-C-j MELTS[J]. Acta Metall Sin, 1986, 22(6): 89-91.

全文: PDF(230 KB)  
摘要: <正> As一向认为是钢铁中的有害元素。除少数耐腐蚀钢种外,脱As是钢铁冶炼的一个问题。欲脱As必先知As在铁液中的热力学行为。文献中只报道过As的活度相互作用系数e_(As)~C,e_(As)~S及e_(As)~N。本文是继续前文研究As在Fe液中的热力学行为,旨在利用下列反应: 3(CaC_2)+2[As]=(Ca_3As_2)+6[C] (1) 求出Fe-As-C-j熔体中的
Abstract:Equilibrium experiments of iron melts containing As and saturated C with CaC_2-CaF_2 slag, which was saturated with CaC_2, were carried out under highly purified Ar atmosphere at 1350, 1425 and 1500℃. The free energy of the reaction 3(CaC_2)+2[As]=(Ca_3As_2)+6[C] is found to be △G°=-88150+29.80T(J), both As and Ca_3As_2 based on the infinitely dilute or 1% by weight solution standard. A plot of 1g fCα_3As_2 νS (%Ca_3As_2) gives values of the activity coefficient of Cα_3As_2. From the experimental equilibrium data of the quarternary system Fe-As-C-j where j=Si, Mn, P, values of 1g f_(As)~j can thus be evaluated. The interaction coefficients of the activity of As in iron melts e_(As)~j, are thus obtained as follow: e_(As)~(Si) e_(As)~(Mn) e_(As)~P 1350℃ 0.064 -0.035 0 1600℃ 0.057 -0.031 0
收稿日期: 1986-06-18     
1 不破祐;藤倉正国;的埸幸雄,铁钢,46(1960) ,235.
2 Banya, S.; Chipman, J,, Trans. Metall. Soc. AIME, 245 (1969) , 133.
3 Schenck, H.; Frohberg, M.G.; Graf, H., Arch. Eisenhuettenwes., 29 (1958) , 673.
4 朱元凯;董元篪;彭(忄育)强;魏寿昆,钢铁,20(1985) ,№10,38.
5 Mitchell, A., Trans. Metall. Soc. AIME, 242 (1968) , 2507.
6 董元篪等、彭(忄育)强、魏寿昆、朱元凯,钢铁,21(1986) ,№10,16.
7 Gmelin-Durrer, Metallurgie des Eisens, Springer-Verlag, Berlin, 1978, Bd. 5a, p. 166a.
8 Neumann, F.; Schenck, H., Arch. Eisenhuettenwes., 30 (1959) , 477.@
No related articles found!