金属学报  1986, Vol. 22 Issue (6): 81-83    
  论文 本期目录 | 过刊浏览 |
含Nb微合金钢中有序NbC的初步研究
雍岐龙;郑鲁;孙珍宝
冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院
ON THE ORDERED NIOBIUM CARBIDE IN MICROALLOY STEELS
by YONG Qilong; ZHENG Lu; SUN Zhenbao (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing)
引用本文:

雍岐龙;郑鲁;孙珍宝. 含Nb微合金钢中有序NbC的初步研究[J]. 金属学报, 1986, 22(6): 81-83.
, , . ON THE ORDERED NIOBIUM CARBIDE IN MICROALLOY STEELS[J]. Acta Metall Sin, 1986, 22(6): 81-83.

全文: PDF(467 KB)  
摘要: <正> 许多研究者采用金属氢化物与石墨反应、区域熔炼或粉末烧结等方法制备MCx相样品,用X光衍射、核磁共振或透射电镜等技术进行研究时发现,在VC_(0.77)-VC_(0.88)之间有一三角系或单斜系的有序V_6C_5相;在VC_(0.87)-VC(0.90)之间有一立方系的有序V_8C_7相;在NbC_(0.67)-NbC_(0.97)之间有一与有序V_6C_5类似的Nb_6C_5相。此外,长时间时效后,在Fe-1V-0.02Nb-0.2C合金中沉淀的碳化钒中发现有序V_6C_5相;在Ni-4V-0.4C合金中发现有序V_6C_5相;在中碳合金钢中发现有序V_6C_5和有序(V,Ti)_6C_5相;在热强钢中发现有序V_8C_7相。
Abstract:The precipitated niobium carbide is revealed to be ordered in ferrite in 3 different microalloyed steels containing Nb about 0.08—0.24%. This ordered niobium carbide may be formulated as Nb_8C_7~′(NbC_(0.875)~′) which is formed by ordered omission of its C atoms. With the reciprocal lattice indexes or orientation relationship of transformation matrix between the ordered niobium carbide and α-Fe, the composite electron diffraction patterns can be conveniently indexed.
收稿日期: 1986-06-18     
1 De Novion, C.H.; Lorenzelli, R.; Costa, P., C. R. Hebd. Seances Acad. Sci., 263 (1966) , 775.
2 Venables, J.D.; Kahn. D.; Lye, R.G., Philos. Mag., 18 (1968) , 177.
3 Froidevaux, C.; Rossier, D., J. Phys. Chem. Solids, 28(1967) , 1197.
4 Kordes, D., Phys. Status Solidi, 26 (1968) , k103.
5 Billingham, J.; Lewis, M. H. 7th Int. Congress for EM, Grenoble 1970, p. 477.
6 Hollox, G.E.; Edington, J. W.; Scarlin, R. B., J. Iron Steel Inst., 209 (1971) , 839.
7 Scarlin, R.B.; Edington, J. W., J. Mater. Sci., 9 (1974) , 1590.
8 Dunlop, G.L.; Porter, D.A., Scand. J. Met., 16 (1977) , 19.
9 董企铭,硕士论文,冶金部钢铁研究总院,1981.
10 雍岐龙,郑鲁,金属学报,20(1984) ,19.
11 Nordberg, H.; Aronsson, B., J. Iron Steel Inst., 206 (1968) , 1263.
12 Nagakura, S.; Oketani, S., Trans. Iron Steel Inst. Jpn., 8 (1968) , 265