| Ni-Be-Ti合金固溶处理参数对β相溶解的影响 |
| 庄应烘;汤广权;荣国器 |
| 广西大学;广西大学;广西大学 |
|
| INFLUENCE OF SOLUTION TREATMENT PARAMETERS ON DISSOLUTION OF β-PHASE FOR Ni-Be-Ti ALLOYS |
| ZHUANG Yinghong; TANG Guangquan; RONG Guoqi (Guangxi University; Nanning) |
引用本文:
庄应烘;汤广权;荣国器. Ni-Be-Ti合金固溶处理参数对β相溶解的影响[J]. 金属学报, 1986, 22(5): 57-62.
,
,
.
INFLUENCE OF SOLUTION TREATMENT PARAMETERS ON DISSOLUTION OF β-PHASE FOR Ni-Be-Ti ALLOYS[J]. Acta Metall Sin, 1986, 22(5): 57-62.
1 Kawacki Berylco Industries Inc., Berylco Nickel Alloys 440, Alloy Digest, Publ. by Eng, Alloys Digest Inc., Upper Montclair, New Jersey, Revised Sept. 1975. 2 村上陽太郎,日本金属学会会报,13(1974) ,479. 3 湯广权;荣国器,卢美德;孙精勤,庄应烘,广西大学学报,待发表. 4 Jahn, E.Z., Z. Metallk., 40 (1949) , 399. 5 Aldinger, F.; Petzow, G., Beryllium Science and Technology, Vol. 1, Eds. Webster, D.; London, G. J., Plenum Press, New York, 1979, p. 235.% |
|