硼在渗层中的行为与渗层淬透性
褚幼义;贺信莱;冯锐林;陈治国;吴锦尧
北京钢铁学院;北京钢铁学院;南昌齿轮厂;南昌齿轮厂;南昌齿轮厂
BEHAVIOUR OF BORON IN CARBONIZED AND CARBONITRIDED CASE AND CASE-HARDENABILITY OF BORON STEEL
CHU Youyi; HE Xinlai (Beijing University of Iron and Steel Technology); FENG Ruilin; CHEN Zhiguo; WU Jinyao (Nanchang Gear Plant)
引用本文:

褚幼义;贺信莱;冯锐林;陈治国;吴锦尧. 硼在渗层中的行为与渗层淬透性[J]. 金属学报, 1986, 22(5): 5-15.
, , , , . BEHAVIOUR OF BORON IN CARBONIZED AND CARBONITRIDED CASE AND CASE-HARDENABILITY OF BORON STEEL[J]. Acta Metall Sin, 1986, 22(5): 5-15.

全文: PDF(1777 KB)  
摘要: 含硼钢渗碳和碳氮共渗时,由于硼与氮及碳之间的相互作用,硼在整个渗层范围内发生明显的再分布。在渗碳层中主要表现为硼在表层富集和次表层内贫化,在碳氮共渗层中主要表现为,在距表面很深的范围内有大量BN形成以及固溶硼量很低的地区发展得很深。 硼的这种再分布对渗层淬透性带来显著影响,渗碳层的淬透性,除了要考虑碳含量的变化以及碳对硼效应的影响外,还要考虑次表层硼贫化的影响。在碳氮共渗层中,大量BN的形成对淬透性有显著的不良影响,固溶硼贫化的作用也表现得更为突出。
Abstract:The B is obviously redistributed in B steel within the whole carbonized and carbonitrided case because of the interaction between B with N and C during carbonizing and carbonitriding. The most of all behaviour of B observed in the carbonized case is the enrichment into the surface layer and the depletion from the sub-layer beneath surface, and in the earbonitrided case is the formation of abundant BN in the wide region from surface and the extension of depleted solution B into deep zone. The redistribution of B is remarkably influenced on the hardenability of the case. The carbonized case hardenability is affected not only by the carbon changed in content and influenced on B hardenability effect, but also by the B depletion in sub-layer. The abundant BN particles with solution B depletion deeply into the interior formed in carbonitrided ease is very harmful to the hardenability.
收稿日期: 1986-05-18     
1 Jatczak, C. F.; Rowland, E.S., Trans. ASM, 45 (1953) , 771.
2 Grange, R.A.; Mitchell, J.B., Trans. ASM, 46 (1954) , 446.
3 关启标;李林,金属学报,1(1956) ,255.
4 Llewellyn, D.T.; Cook, W.T., Met. Technol., 1(1974) . 517.
5 贺信莱;褚幼义;张秀林;余宗森;李秋萍;尹熙光,会属学报,13(1977) ,235.
6 He, X.L.; Chu, Y.Y., J. Phys, D: Appl. Phys., 16 (1983) , 1145.
7 Rahrer, G.D.; Armstrong, C.D., Trans. ASM, 40 (1948) , 1099.
8 Grossman, M.A., Trans. AIME, 150 (1942) , 227.
9 Kunze, C.T.; Keil, G., Boron in Steel, Eds. Banerji, S.K.; Morral, J.E., AIME, 1980, p. 106.
10 Chatterjee-Fischer, R., Metall. Trans., 9A (1978) , 1553.
11 北京齿轮厂热处理车间;北京钢铁学院金相专业北齿实践队,金属热处理,(1977) ,№ 3. 13.
12 洪觉宏,金属热处理,(1981) ,№ 8,35.
13 Kawasaki, S.; Hishinma, A.; Nagasaki, R., J. Nucl. Mater., 39 (1971) , 166.
14 Smithells, C.J., Metals Reference Book, 5th ed., 1976