| 奥氏体晶界迁移过程的研究 |
| 胡德林;刘智恩 |
| 西北工业大学;西北工业大学 |
|
| ON THE MIGRATION OF AUSTENITE GRAIN BOUNDARY |
| by HU Delin; LIU Zhi'en (North-western Polytechnical University; Xi'an) |
引用本文:
胡德林;刘智恩. 奥氏体晶界迁移过程的研究[J]. 金属学报, 1986, 22(4): 56-152.
,
.
ON THE MIGRATION OF AUSTENITE GRAIN BOUNDARY[J]. Acta Metall Sin, 1986, 22(4): 56-152.
1 Gladman, T.; Pickering, F.B., J. Iron Steel Inst.,205 (1967) , 653 2 Caha, R.W., Physical Metallurgy, capt. 19, 2nd ed. North-Holland, Amsterdam, 1970, p. 1181. 3 肖纪美,职任涛,刘昌其,特殊钢,(1982) .№6,1. 4 胡德林;张明义;刘智恩;黄伟涛,特殊钢,(1982) ,№6,24. |
|