| 非晶态合金(Fe_(1-x)V_x)_(84)B_(16)的低温电阻率反常 |
| 陈金昌;詹文山;沈保根;赵见高;司红 |
| 北京师范学院物理系;中国科学院物理研究所;中国科学院物理研究所;中国科学院物理研究所;冶金工业部钢铁研究总院 |
|
| LOW TEMPERATURE RESISTIVITY ANOMALY FOR AMORPHOUS (Fe_(1-x)V_x))_(84)B_(16) ALLOYS |
| by CHEN Jinchang (Beijing Teachers' College); ZHAN Wenshan; SHEN Baogen; ZHAO Jiangao (Institute of Physics; Academia Sinica; Beijing); SI Hong (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
引用本文:
陈金昌;詹文山;沈保根;赵见高;司红. 非晶态合金(Fe_(1-x)V_x)_(84)B_(16)的低温电阻率反常[J]. 金属学报, 1986, 22(4): 121-124.
,
,
,
,
.
LOW TEMPERATURE RESISTIVITY ANOMALY FOR AMORPHOUS (Fe_(1-x)V_x))_(84)B_(16) ALLOYS[J]. Acta Metall Sin, 1986, 22(4): 121-124.
1 詹文山;沈保根;郭慧群,低温物理,5(1983) ,№2,91. 2 沈保根;詹文山;章志英;吴宗林,金属学报,20(1984) ,B164. 3 陈金昌;詹文山;沈保根;赵见高,乐观,物理学报,35(1986) ,25 4 Chan, W.S.; Shen, B.G.; Lo, H.Y.; Yu, B.L., Proc. 4th Int. Conf. on Rapidly Quenched Metals, (Sendai, 1981) , Eds. Masumoto, T.; Suzuki, K., JIM, 1982, p. 1137. 5 汪仲诚;刘福绥,物理学报,32(1983) ,33. 6 李正中;胡筱欣;王金才,物理学报,34(1985) ,145. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|