| 超高强度钢中的(M-A)组织和贝氏体 |
| 钟炳文;宋宇文 |
| 北京航空材料研究所;北京航空材料研究所 |
|
| THE M-A STRUCTURE AND BAINITE IN ULTRA HIGH STRENGTH LOW ALLOY STEELS |
| by ZHONG Bingwen; SONG Yuwen (Institute of Aeronautical Materials; Beijing) |
引用本文:
钟炳文;宋宇文. 超高强度钢中的(M-A)组织和贝氏体[J]. 金属学报, 1986, 22(4): 11-144.
,
.
THE M-A STRUCTURE AND BAINITE IN ULTRA HIGH STRENGTH LOW ALLOY STEELS[J]. Acta Metall Sin, 1986, 22(4): 11-144.
1 Thomas. G., Metall, Trans., 9A (1978) , 439. 2 Marasimha Rao, B.V.; Thomas, G., Metall. Trans., 11A (1980) , 441. 3 73 (1950) , 1161. 4 Huang, D.-H.; Thomas, G., Metall. Trans., 8A (1977) , 1661. 5 Jack, K.H., J. Iron Steel Inst., 169 (1951) , 26. 6 Sarikaya, M.; Thingan, A, K.; Thomas, G., Metall Trans., 14A (1983) , 1121. 7 Aaronson, H.I.; Plichta, M.R.; Franti, G.W.; Russell, K.L., Metall. Trans., 9A (1978) , 363. 8 李春志,物理学报,28(1979) ,314.? |
|