氢对Ti-15Mo合金弹性模量及原子间结合能的影响
万晓景;杨柯;曹名洲
中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所
EFFECT OF HYDROGEN ON YOUNG' S MODULUS AND COHESIVE ENERGY OF Ti-15Mo ALLOY
by WAN Xiaojing; YANG Ke; CAO Mingzhou (Institute of Metal Research; Academia Sinica; Shenyang)
引用本文:

万晓景;杨柯;曹名洲. 氢对Ti-15Mo合金弹性模量及原子间结合能的影响[J]. 金属学报, 1986, 22(3): 9-14.
, , . EFFECT OF HYDROGEN ON YOUNG' S MODULUS AND COHESIVE ENERGY OF Ti-15Mo ALLOY[J]. Acta Metall Sin, 1986, 22(3): 9-14.

全文: PDF(497 KB)  
摘要: 利用声频共振法及静态方法研究了氢对β型Ti-15Mo合金弹性模量的影响。结果表明氢连续降低合金的弹性模量。弹性模量的降低不是氢化物的形成或充氢造成的损伤所致,且其降低与恢复完全是可逆的。利用离子探针质谱微分析仪测量了不同氢含量试样之间结合能的差异。结果表明固溶氢显著降低合金的结合能。实验结果可由金属的弱键理论加以解释。氢降低弹性模量是其降低晶格结合能的结果。本实验事实可作为弱键理论的一个直接验证。
Abstract:The effect of hydrogen on the Young's modulus for β-titanium alloy Ti-15Mo was investigated by both acoustic resonance and static methods. Results show that the Young's modulus is continuously reduced by hydrogen. It seems to be not the result of hydride formation and damage caused by hydrogen charging, and the decrease of modulus induced by hydrogen and its recovery are reversible entirely. The difference of cohesive energy iamong the specimens charged with various hydrogen contents was measured by ion microprobe mass analyzer. The cohesive energy is found to be significantly lowered by dissolved hydrogen. An explanation of the experimental results may be given by the decohesion theory of hydrogen embrittlement. The Young's modulus decrease of the alloy induced by hydrogen may be attributed at least partly to the lowering of cohesive energy of the lattice, and this study may be considered as a verification of the decohesion theory.
收稿日期: 1986-03-18     
1 Paton, N.E.; Buck, O., Effects of Hydrogen on Behavior of Materials, AIME, New York, 1976, p. 83.
2 Paton, N.E.; Spurling, R.A., Hydrogen Effects in Metals, 1983, p. 269.
3 万晓景;高耕宇;秦荣士;赵吉祥,材料科学进展--纪念李薰逝世三周年,科学出版社出版,1986.
4 Woda, M.; Uemori, R.; Nishikawa, O., Surf. Sci, 134 (1983) , 17.
5 李昕,金属材料研究,3 (1975) ,433.
6 Troiano, R., Trans. ASM, 52 (1960) , 54.Z