金属学报  1986, Vol. 22 Issue (3): 56-62    
  论文 本期目录 | 过刊浏览 |
Cu-26Zn-4Al形状记忆合金马氏体相变晶体学 Ⅱ.群论的应用
朱伟光;陈伟业;徐祖耀
上海交通大学;上海交通大学;上海交通大学
CRYSTALLOGRAPHY OF MARTENSITIC TRANSFORMATION IN A Cu-26Zn-4Al SHAPE MEMORY ALLOY Ⅱ. Application of Group Theory
by ZHU Weiguang; CHEN Weiye; XU Zuyao(T.Y. Hsu) (Shanghai Jiaotong University)
引用本文:

朱伟光;陈伟业;徐祖耀. Cu-26Zn-4Al形状记忆合金马氏体相变晶体学 Ⅱ.群论的应用[J]. 金属学报, 1986, 22(3): 56-62.
, , . CRYSTALLOGRAPHY OF MARTENSITIC TRANSFORMATION IN A Cu-26Zn-4Al SHAPE MEMORY ALLOY Ⅱ. Application of Group Theory[J]. Acta Metall Sin, 1986, 22(3): 56-62.

全文: PDF(516 KB)  
摘要: 本文试图用群论的理论分析,探讨Cu-Zn-Al合金马氏体相变的晶体学性质:由群的表示理论找得诱导该合金B_2结构母相β→非规则9R马氏体的不可约表示;由群论讨论该合金马氏体相变具有24个变态的可能性,找出由组态组成的自协调组织的对称性群D_2h,揭示了变态间的对称联系和分布规律。
Abstract:From group theory, the irreducible representation and the 24 variants associated with the martensitic transformation of a Cu-26Zn-4Al alloy are obtained. The self-accommodating group is found to be D_(2h) and the symmetry in one and the set of self-accommodating group are analyzed.
收稿日期: 1986-03-18     
1 Cahn, J.W., Acta Metall., 25 (1977) , 721.
2 Cahn, J.W.; Kalonj, G., Proc. Int. Conf. Solid-Solid Phase Transformations, Eds, Aaronson, H.I., et al., TMS-AIME, 1981, p. 3.
3 Pottier, R.; Gratias, D., Proc. Int. Conf. on Martensitic Transformations, Eds. Delaey, L.; Chandrasekaran, M., J. Phys., C-4, Supplement an №12, Dec. 1982, C4-17.
4 Landau.L.D.;Lifshitz,E.M.,统计物理学,杨训愷译,人民教育出版社,1964,p.535.
5 Lyubarskii,G.Ya.,群论及其在物理学中的应用,数学研究所译,科学出版社,1958. p.102.
6 陶瑞宝,物理学进展,3 (1982) ,189.
7 Bling,R.;zeks,B.,铁电体和反铁电体的软模,刘长乐等译,科学出版社,1981,p.63.
8 Saburi, T.; Wayman, C.M., Acta Metall., 28 (1980) , 15.
9 Saburi, T.; Kato, S.N.; Takata, K., J. Less-Common Met., 50 (1976) , 223.
10 Saburi, T.; Wayman, C.M., Acta Metall., 28 (1980) , 1.
11 Perkins, J., Metallography, 7 (1974) , 345.
12 唐有祺,对称性原理,科学出版社,1979.
13 Koster.G.F.,物理译丛(固体物理),(1965) .№2,6.
14 Kovalev, O.V., Irreducible Representations of the Space Groups, Gordon & Breach Science Publ., New York, 1965.
15 Sabari, T.; Wayman, C.M., Acta Metall., 27 (1979) , 979.
No related articles found!