| 熔融石英颗粒复合材料的断裂行为 |
| 王润泽;刘延伶 |
| 冶金部洛阳耐火材料研究所;冶金部洛阳耐火材料研究所 |
|
| FRACTURE BEHAVIOUR OF FUSED QUARTZ PARTICULATE COMPOSITES |
| by WANG Runze; LIU Yanling (Luoyang Institute of Refractory Research) |
引用本文:
王润泽;刘延伶. 熔融石英颗粒复合材料的断裂行为[J]. 金属学报, 1986, 22(3): 117-123.
,
.
FRACTURE BEHAVIOUR OF FUSED QUARTZ PARTICULATE COMPOSITES[J]. Acta Metall Sin, 1986, 22(3): 117-123.
1 Hasselman, D.P.H., J. Am. Ceram. Soc., 46 (1963) , 535. 2 Hasselman, D.P.H., J. Am. Ceram. Soc., 52 (1969) , 600. 3 Hasselman, D.P.H., J.Am Ceram. Soc., 49 (1966) , 68. 4 Lange, F.F., Philos. Mag., 22 (1970) , 983. 5 Green, D.J.; Nicholson, P.S.; Embury, J.D., J.Mater. Sci, 14 (1979) , 1413. 6 Khaund, A.K.; Nicholson, P.S., J.Mater. Sci., 15 (1980) , 177. 7 楼福珍;钮雁南;邹甫俊,耐火材料,(1980) ,№6,33. 8 Nakayama, J., J. Am. Ceram. Soc., 48 (1965) , 583. 9 Lange, F.F.. J.Am. Ceram. Soc., 54 (1971) , 614. 10 Uchno, J.J.; Bradt, R.C.; Hasselman, D.P.H., Am. Ceram. Soc, Bull., 55 (1976) , 665. 11 Nakayama, J.; Ishizuka, M., Am. Ceram. Soc. Bull, 45 (1966) , 666.5 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|