| 高温合金中Cr_7C_3相的晶体结构与孪晶 |
| 李玉清;刘锦岩 |
| 大冶钢厂钢铁研究所;大冶钢厂钢铁研究所 |
|
| CRYSTALLINE STRUCTURE AND TWIN OF Cr_7 C_3 IN SUPERALLOYS |
| LI Yuqing; LIU Jinyan (Research Institute of Daye Steel Works) |
引用本文:
李玉清;刘锦岩. 高温合金中Cr_7C_3相的晶体结构与孪晶[J]. 金属学报, 1986, 22(1): 50-63.
,
.
CRYSTALLINE STRUCTURE AND TWIN OF Cr_7 C_3 IN SUPERALLOYS[J]. Acta Metall Sin, 1986, 22(1): 50-63.
1 Westgren, A., Jernkontorets Ann., 119 (1935) , 231. 2 Herbstein, F.H.; Snyman, J.A., Inorg. Chem., 3 (1964) , 894. 3 Fyuchart, R.; Senateur, J.-P.; Bouchaud, J.-P,; Michel, A., C.R. Hebd. Seances Acad. Sci., 260 (1965) , 913. 4 Fruchart, R.; Rouault, A., Ann. Chim., (Paris), 4 (1969) , 143. 5 桶谷繁雄,電子線回折金属炭化物研究,株式会社,东京,1971,p.217. 259.M |
|