| 某些非晶态合金的电阻率-温度特性 |
| 冯本政;杨汝森 |
| 昆明贵金属研究所;昆明贵金属研究所 |
|
| TEMPERATURE DEPENDENCE OF ELECTRICAL RESISTIVITY OF SOME AMORPHOUS ALLOYS |
| FENG Benzheng;YANG Rusen Institute of Precious Metals Kunming |
引用本文:
冯本政;杨汝森. 某些非晶态合金的电阻率-温度特性[J]. 金属学报, 1985, 21(4): 89-94.
,
.
TEMPERATURE DEPENDENCE OF ELECTRICAL RESISTIVITY OF SOME AMORPHOUS ALLOYS[J]. Acta Metall Sin, 1985, 21(4): 89-94.
1 Gallagher,B.L.;Greig,D.;J.Phys.,F.12(1982) ,1721. 2 Budhani,R.C.;Goel,T.C.;Chopra,K.L.,J.Phys.,F,13(1983) ,129. 3 Bushow,K.H.J.;Beekman,N.M.,Phys.Rev.,B,19(1979) ,3843. 4 Fritsch,G.;Willer,J.;Luescher,E.,J.Non-Cryst.Solids,46(1981) ,321. 5 Hwang,C.H.,J.Less-Common Met.,86(1982) ,187. 6 冯本政;朱应华;杨汝森,金属学报,20(1984) ,B 224. |
|