| 第三长周期过渡金属对PdSi_(16.5)非晶态合金延脆转变性能的影响 |
| 郑云;宁远涛 |
| 昆明贵金属研究所;昆明贵金属研究所 |
|
| INFLUENCE OF TRANSITION METALS OF THE THIRD LONG PERIOD ON DUCTILE-BRITTLE TRANSFORMATION OF PdSi_(16.5)GLASS |
| ZHENG Yun;NING Yuantao Institute of Precious Metals;Kunming |
引用本文:
郑云;宁远涛. 第三长周期过渡金属对PdSi_(16.5)非晶态合金延脆转变性能的影响[J]. 金属学报, 1985, 21(4): 113-119.
,
.
INFLUENCE OF TRANSITION METALS OF THE THIRD LONG PERIOD ON DUCTILE-BRITTLE TRANSFORMATION OF PdSi_(16.5)GLASS[J]. Acta Metall Sin, 1985, 21(4): 113-119.
1 Walter,J.W.;Luborsky,F.E.,Mater.Sci Eng.,33(1978) ,91. 2 Liebermann,H.H.;Luborsky,F.E.,Acta Metall.,29(1981) ,1413 3 宁远涛;郑云;祁更新,金属学报,19(1983) ,B 209. 4 Luborsky,F.E.;Walter,J.L.,J.Appl.Phys.,47(1976) ,3648. 5 Masumoto,T.;Maddin,R.,Acta Metall.,19(1971) ,725. 6 Chen,H.S.,J.Non-Crystal Solids,27(1978) ,257. 7 Chen,H.S.,Mater.Sci.Eng.,26(1976) ,79. 8 Freed,R.L.;Vander Sande,J.B.,Acta Metall.,28(1980) ,103.a |
|