| 工业Al-Cu-Mg合金中的Portevin-Le Chatelier效应 |
| 张彩碚;王洪祥;王继尧;赖祖涵 |
| 东北工学院;东北工学院;东北工学院;东北工学院 |
|
| PORTEVIN-LE CHATELIER EFFECT IN COMMERCIAL AI-Cu-Mg ALLOY |
| ZHANG Caipei;WANG Hongxiang;WANG Jiyao;LAI Zuhan Northeast Institute of Technology;Shenyang |
引用本文:
张彩碚;王洪祥;王继尧;赖祖涵. 工业Al-Cu-Mg合金中的Portevin-Le Chatelier效应[J]. 金属学报, 1985, 21(4): 1-7.
,
,
,
.
PORTEVIN-LE CHATELIER EFFECT IN COMMERCIAL AI-Cu-Mg ALLOY[J]. Acta Metall Sin, 1985, 21(4): 1-7.
1 Van Den Beukel,A.,Phys.Status Solidi,(a)30(1975) ,197. 2 塚田晴一;井上稔;高桥明男,塑性加工,15(1974) ,526. 3 Couchman,P.R.;Reynolds,C.L.,Jr.,Philos.Mag.,34(1976) ,327. 4 Miura B,Mechanical Behavior of Materials,Proc.of the Int.Conf.on Mechanical Behavior of Materials,Vol.1,JSMS,1972,p.128. 5 Mukherjee,K.;May,T.;D' Antonic,C.;Maciag,R.J.,Metall.Trans.1(1970) ,3233. 6 Kimura,H.;Kimura,A.;Hasiguti,R.R.,Acta Metall.,10(1962) 607. 7 King,J.E.;You,C.P.;Knott,J.F.,Acta Metall.,29(1981) ,1553. |
|