| 塑性和超塑性材料m-n-δ关系的简化表达式 |
| 连建设;张吉人 |
| 吉林工业大学;哈尔滨工业大学 |
|
| A SIMPLIFIED EXPRESSION OF m-n-δ RELATIONS FOR MATERIALS WITH PLASTICITY OR SUPERPLASTICITY |
| LIAN Jianshe Jilin Institute of Technology;Changchun;ZHANG Jiren Harbin Institute of Technology |
引用本文:
连建设;张吉人. 塑性和超塑性材料m-n-δ关系的简化表达式[J]. 金属学报, 1985, 21(2): 118-123.
,
.
A SIMPLIFIED EXPRESSION OF m-n-δ RELATIONS FOR MATERIALS WITH PLASTICITY OR SUPERPLASTICITY[J]. Acta Metall Sin, 1985, 21(2): 118-123.
1 Backofen,W.A.;Turner,I.R.;Avery,D.H.,ASM Trans.Q.,57(1964) ,980. 2 Hart,E.W.,Acta Metall.,15(1967) ,351. 3 Woodford,D.A.,ASM Trans.Q.,62(1969) ,291. 4 Morrison,W.B.,Trans.Metall.Soc.AIME,242(1968) ,2221. 5 Avery,D.H.;Stuart,J.M.,14th Sagamove Army Materials Research Conf.Raquette Lake,N.Y.1967. 6 Ghosh,A.K.;Ayers,R.A.,Metall.Trans.,A7(1976) ,1589. 7 Hutchinson,J.W.;Neale,K.W.,Acta Metall.,25(1977) ,839. 8 Ghosh,A.K.,Acta Metall.,25(1977) ,1413. 9 Nichols,F.A.,Acta Metall,28(1980) ,663. 10 连建设,机械工程学报,18(1982) ,№4,21. 11 Lin.I.H.;Hirth,J.P.;Hart,E.W.,Acta Metall,29(1981) ,819. 12 Considère,A.,Ann.Ponts Chaussees,6(1885) ,574. 13 Hart,E.W.,Acta Metall.,18(1970) ,599. 14 Ferron,G.;Mliha-Touati,M.,Scr.Metall.,16(1982) ,911. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|