| 对压力下结晶形核率的理论计算 |
| 齐丕骧 |
| 内蒙古金属材料研究所 |
|
| AN EXPRESSION FOR NUCLEATION RATE OF CRYSTALLIZATION UNDER PRESSURE |
| QI Pixiang (Nei Monggol Institute of Metallic Materials; Baotou) (Manuscript received 8 November; 1982; revised manuscript 31 March; 1984) |
引用本文:
齐丕骧. 对压力下结晶形核率的理论计算[J]. 金属学报, 1984, 20(6): 465-470.
.
AN EXPRESSION FOR NUCLEATION RATE OF CRYSTALLIZATION UNDER PRESSURE[J]. Acta Metall Sin, 1984, 20(6): 465-470.
1 #12 2 西田義则;松原弘美;白柳格;鈴木鎮夫,日本金属学会会報,19(1980) ,895. 3 Davies, G. J., Solidification and Casting, Applied Science Publ. London, 1973, p.18. 4 Yoshinori Nishida; Hiromi Matsubara, Z. Metallk., 71 (1980) , №3, 193. 5#12 6 #12 7 Robert, C. W., CRC Handbook of Chemistry and Physics, CRC Press, Cleveland Ohio, 1977-1978, 58th ed. p. C-192. 8#12 |
|