| 钛合金热稳定性研究 Ⅰ.Ti_3X相形成的电子浓度规律 |
| 李东;刘羽寅;万晓景 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| ON THE THERMAL STABILITY OF Ti ALLOYS I. The Electron Concentration Rule for Formation of Ti_3X-Phase |
| LI Dong; LIU Yuyin; WAN Xiaojing (Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 4 November; 1983; revised manuscript 29 February;1984) |
引用本文:
李东;刘羽寅;万晓景. 钛合金热稳定性研究 Ⅰ.Ti_3X相形成的电子浓度规律[J]. 金属学报, 1984, 20(6): 375-484.
,
,
.
ON THE THERMAL STABILITY OF Ti ALLOYS I. The Electron Concentration Rule for Formation of Ti_3X-Phase[J]. Acta Metall Sin, 1984, 20(6): 375-484.
1 Blackburn, M. J., Trans. Metall. Soc. AIME, 239 (1967) , 1200. 2 Anderko, K., Z. Metallk., 49(1958) , 165. 3 Pietrokowsky, P.; Frink, E., Trans. ASM, 49(1957) , 339. 4 Shamblen, C. E., Metall. Trans., 2(1971) , 277. 5 Mendiratta, M. G.; Chakrabarti, A. K.; Roberson, J. A., Metall. Trans., 5 (1974) , 1949. 6 Shamblen, C. E.; Redden, T. K., Metall. Trans., 3 (1972) , 1299. 7 Soltis, P. J., Trans. Metall. Soc. AIME, 233 (1965) , 903. 8 Erdeman, V. J.; Ross, E. W., The Science, Technology and Application of Titanium, Proc. of lst Int. Conf. on Titanium, Eds. Jaffee, R. I.; Promisel, N. E., Pergamon, London, 1970, p. 829. 9 McQuillan, A. D.; Margolin, H.; Collings, E. W., Titanium Science and Technology, Proc. of 2nd Int. Conf. on Titanium, Eds, Jaffee, R. I.; Burte, H. M., Pergamon, London, 1973, p. 969. 10 Smallman R. E., Modern Physical Metal, 3rd ed., Butterworths, London, 1970, p. 140. 11 Jones, H., Proc. R. Soc., 144 (1934) , 225; Proc. Phys. Soc., 49 (1937) , 250. 12 Engel, N., Trans. ASM, 57 (1964) , 610. 13 Hume-Rothery, W.; Irving, H. M.; Williams, R. J. P., Proc. R. Soc., A208(1951) , 431. 14 Fisher, E. S.; Dever, D., Acta Metall., 18 (1970) , 265. 15 Das, D. K.; Rideout, S. P.; Beck, P. A., Trans. AIME, 194 (1952) , 1071. 16 Sagel, K.; Schulz, E.; Zwicker, U., Z. Metallk., 47 (1956) , 529. 17 Ence, E.; Margolin, H., Trans. Metall. Soc. AIME, 221 (1961) , 151. 18 Tsujimoto, T.; Adachi, M., J. Inst. Met., 94 (1966) , 358. 19 Crossley, F, A., Trans. Metall. Soc. AIME, 236 (1966) , 1174. 20 Blackburn, M. J., Trans. Metall. Soc. AIME, 239 (1967) , 1200. 21 #12 22 Blackburn, M. J., ASM Trans. Q., 59 (1966) , 694. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|