| 压应力条件下缺口产生疲劳裂纹的研究 |
| 刘天化;褚武扬;肖纪美;金连强 |
| 首都钢铁公司设计院;北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| FATIGUE-CRACK INITIATED FROM NOTCH TIP UNDER CYCLIC COMPRESSIVE LOAD |
| LIU Tianhua (Design Institute of Shoudu Iron arid Steel Co.; Beijing); CHU Wuyang; XIAO Jimei; JIN Lianqiang (Beijing University of Iron and Steel Technology)(Manuscript received 26 March; 1983; revised manuscript 27 December; 1983) |
引用本文:
刘天化;褚武扬;肖纪美;金连强. 压应力条件下缺口产生疲劳裂纹的研究[J]. 金属学报, 1984, 20(5): 341-347.
,
,
,
.
FATIGUE-CRACK INITIATED FROM NOTCH TIP UNDER CYCLIC COMPRESSIVE LOAD[J]. Acta Metall Sin, 1984, 20(5): 341-347.
1 Reid, C. N. Williams, K.; Hermann, R., Fatigue Eng. Mater. Struct., 1(1979) . 267. 2 褚武扬编著,断裂力学基础,科学出版社,1979,p.116. 3 姚京;褚武扬;肖纪美,金属学报,19(1983) ,A445. 4 Chu W. Y. (褚武扬); Ma R. T. (马若涛); Hsiao C. M. (肖纪美), Scr. Met., 18(1984) , 579. 5 Chu W. Y. (褚武扬); Jing Y. (姚京); Hsiao C. M. (肖纪美), Corrosion, 40(1984) , 302.W |
|