| Nb对Ni-Cr-Ti型变形高温合金稳态蠕变行为的影响 |
| 郭恩才;韩芷元;于树有 |
| 冶金工业部钢铁研究总院;齐齐哈尔钢厂研究所;齐齐哈尔钢厂研究所 |
|
| INFLUENCE OF Nb ON STEADY-STATE CREEP BEHAVIOUR OF Ni-Cr-Ti TYPE WROUGHT SUPERALLOY |
| GUO Encai (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Belling); HAN Zhiyuan; YU Shuyou(Research Institute of Qiqihar Steel Works)(Manuscript received 17 August; 1982; revised manuscript 26 August; 1983) |
引用本文:
郭恩才;韩芷元;于树有. Nb对Ni-Cr-Ti型变形高温合金稳态蠕变行为的影响[J]. 金属学报, 1984, 20(5): 305-312.
,
,
.
INFLUENCE OF Nb ON STEADY-STATE CREEP BEHAVIOUR OF Ni-Cr-Ti TYPE WROUGHT SUPERALLOY[J]. Acta Metall Sin, 1984, 20(5): 305-312.
1 Guo, E. C.; Ma, F. J., Superalloys 1980, Proc. of the Fourth Int. Syrup. on Superalloys, Eds. Tien, J. K.; Wlodek, S. T.; Morrow, H., IlI, et al., ASM, Metals Park, Ohio, 1980, p. 431. 2 陈篪;邓枝生;吴伯群;丁树深,物理学报,23(1974) ,69. 3 Ajaja, O.; Howson, T. E.; Purushothaman, S.; Tien, J. K., Mater. Sci. Eng., 44(1980) , 165. 4 Purushothaman, S.; Tien, J. K., Acta Metall., 26(1978) , 519. 5 Marcinkowrki, M. J. et al., Acta Metall., 9(1961) , 129.E |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|