A NEW SPHEROIDIZATION PROCESS FOR HIGH-SULPHUR MOLTEN IRON |
ZHU Yuanka; PENG Yujiang; HONG Yanruo; SU Liuji; YU Xuebin (Beijing University of Iron and Steel Technology) (Manuscript received 7 March; 1983; revised manuscript 31 October; 1983) |