| Fe-C马氏体价电子结构分析 |
| 张瑞林;余瑞璜 |
| 吉林大学及暨南大学;吉林大学及暨南大学 |
|
| AN ANALYSIS OF VALENCE ELECTRON STRUCTURE OF Fe-C MARTENSITE |
| ZHANG Ruilin; YU Ruihuang (S. H. Yü) (Department of Physics; Jilin University; Changchun) (Manuscript received 27 May; 1983) |
引用本文:
张瑞林;余瑞璜. Fe-C马氏体价电子结构分析[J]. 金属学报, 1984, 20(4): 279-285.
,
.
AN ANALYSIS OF VALENCE ELECTRON STRUCTURE OF Fe-C MARTENSITE[J]. Acta Metall Sin, 1984, 20(4): 279-285.
1 Cohen,M.,Fandamentals of Martenstitic Reaction,中美冶金学术年会报告,北京,1981. 2 徐祖耀,马氏体相变与马氏体,科学出版社,1980. 3 余瑞璜,科学通报,23(1978) ,217. 4 余瑞璜,吉林大学自然科学学报,(1979) ,№ 4,54. 5 余瑞璜,科学通报,26(1981) ,206. 6 Pearsen, W. B., A Handbook of Lattice Spacings and Sturctures of Metals and Alloys, Pergamon Press, New York, 1958, p. 121. 7 De Cristofaro, N.; Kaplow, R., Metall. Trans., 8A (1977) , 35. 8 Choo, W. K.; Kaplow, R., Acta. Metall., 21 (1973) , 725. 9 余瑞璜,金属学报,18(1982) ,336. 10 Kurdjumov, G. V.; Khachaturyan, A. G., Acta Metall., 23 (1975) , 1077. 11 Pearsen, W. B., A Handbook of Lattice Spacings and Structures of Metals and Alloys, Pergamon Press, New York, 1958, p. 927. 12 余瑞璜,γ,γ’,ε,δ-Fe和Fe_3Si,Fe_4N,FeP的价电子结构分析,待发表. 13 Yensen, T. D., Trans. ASM, 27 (1939) , 797. 14 袁祖奎,Fe-Cr“σ相”价电子结构的分析,待发表. 15 余瑞璜,渗碳体(Fe_3C)价电子结构分析,待发表.s |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|