|
|
|
| 40Mn钢拉伸形变观察与分析 |
| 刘禹门;杨桂应 |
| 西安交通大学;西安交通大学 |
|
| EFFECT OF ELONGATION ON DISLOCATION STRUCTURE AND CRACK INITIATION OF HARDENED AND TEMPERED 40Mn STEEL |
| LIU Yumen; YANG Guiying (Xi'an Jiaotong University) (Manuscript received 30 July; 1983; revised manuscript 10 October; 1983) |
引用本文:
刘禹门;杨桂应. 40Mn钢拉伸形变观察与分析[J]. 金属学报, 1984, 20(4): 242-381.
,
.
EFFECT OF ELONGATION ON DISLOCATION STRUCTURE AND CRACK INITIATION OF HARDENED AND TEMPERED 40Mn STEEL[J]. Acta Metall Sin, 1984, 20(4): 242-381.
1 Thomas, G., Metall. Trans., 9A (1978) , 439. 2 Nutting, J., J. Iron Steel Inst., 207 (1969) , 872. 3 Speich, G. R., Trans. Metall. Soc. AIME, 245 (1969) , 2553. 4 Tekin, E.; Kelly, P. M., Precipitation From Iron-Base Alloys, Speich, G. R.; Clark, J. B. Eds., Gordon and Breach, New York, 1965, p. 173. 5 Winchell, P. G.; Cohen, M., ASM Trans. Q., 55 (1962) , 347. 6 Kurdjumov, G. V., J. Iron Steel Inst., 195 (1960) , 26. 7 Roberts, C. S.; Averbach, B. L.; Cohen, M., Trans. ASM, 45 (1953) , 576. 8 Honeycombe, R. W. K.; Steels Microstructure and Properties, Edward Arnold, London, 1981. 9 Picketing, F. B., Physical Metallurgy and the Design of Steels, Appl. Sci. Publ., Barking, Essex, Engl., 1978. 10 Honeycombe, R. W. K., Structure and Strength of Alloy Steels, Climax Molybdenum Co., London, 1973. 11 刘禹门,金属热处理学报,3(1982) ,№ 1,1. 12 Keh, A. S.; Spitzig, W. A.; Nakada, Y., Philos. Mag., 23 (1971) , 829. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|