| 用控制柔度法研究高温低循环疲劳裂纹扩展规律 |
| 王栓柱;迟书耀;耿刚强 |
| 西安航空发动机厂;西安航空发动机厂;西安公路学院 |
|
| INVESTIGATION ON LCF CRACK GROWTH RATE WITH CONTROLLING DEFLECTION AT HIGH TEMPERATURE |
| by WANG Shuanzhu; CHI Shuyao (Xi'an Aeroengine Factory); GENG Gangqiang (Xi'an Highway Institute) (Manuscript received 3 October; 1982; revised manuscript 5 August; 1983) |
引用本文:
王栓柱;迟书耀;耿刚强. 用控制柔度法研究高温低循环疲劳裂纹扩展规律[J]. 金属学报, 1984, 20(2): 83-210.
,
,
.
INVESTIGATION ON LCF CRACK GROWTH RATE WITH CONTROLLING DEFLECTION AT HIGH TEMPERATURE[J]. Acta Metall Sin, 1984, 20(2): 83-210.
1 Chell, G. G., Colloquium on Fracture, 3rd Fracture & Fatigue, Elasto-Plasticity, Thin-Sheet and Micro-Mechanism Problems, London, 1980, p3-12. 2 Muscati, A., Fracture, 3(1977) , 149. 3 Dowling, N. E., Mechanics of Crack Growth, ASTM, STP, 590,(1976) , p. 82-103. 4 Schwalbe, K. H.; Hellman, D., J. Test. Eval., 9(1981) ,№. 3, 218. 5 Rice, J. R., Progress in Flaw Growth and Fracture Toughness, ASTM, STP, 536, (1973) , p. 231. 6 大路清嗣;小仓敬二:久保司郎,机械の研究,31(1979) ,№.1,33. 7 Dowling, N. E., Crack and Fracture, ASTM, STP 601, (1976) , p. 19-32. 8 Fedderson, C. E., Discussion in Planstrain Crack Toughness Testing of Metallic Materials, ASTM, STP, 410, (1973) , p. 77. 9 陈箎:蔡其巩:王仁智,工程断裂力学,(上册),国防工业出版社,1979,p.368. 10 平修二;田中啓介,小川茂,材料,26(1977) ,№.280,p.93. 11 刘绍伦;谢济洲;未发表资料,1981. 12 Wang Shaunzhu; Yank Cheng; Kang Maokung, Eng. Frac. Mech., 4(1983) . 13 Mowbray, D. E., Crack and Fracture, ASTM, STP, 601, (1976) , p 33. 14 Gabrielli, F.; Pelloux, R. N., Metall. Trans., 13A(1982) , 1083. 15 Chen, I-W; Argon, A. S., Acta Metall., 29(1981) , 1321. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|