| 疲劳裂纹扩展机制和塑性区的研究 |
| 邓蓉英;李禾;于桂清 |
| 中国科学院力学研究所;中国科学院力学研究所;中国科学院力学研究所 |
|
| STUDY OF PLASTIC ZONE AND FATIGUE CRACK PROPAGATION MECHANISM |
| by DENG Rongying; LI He; YU Guiqing (Institute of Mechanics; Academia Sinica; Beijing) (Manuscript received 1 March; 1983; revised manuscript 5 August; 1983) |
引用本文:
邓蓉英;李禾;于桂清. 疲劳裂纹扩展机制和塑性区的研究[J]. 金属学报, 1984, 20(2): 76-209.
,
,
.
STUDY OF PLASTIC ZONE AND FATIGUE CRACK PROPAGATION MECHANISM[J]. Acta Metall Sin, 1984, 20(2): 76-209.
1 Klesnil, M.; Lukas, P., Int. Conf. on Fracture, 2nd, Brighton, 1969, Fracture 1969, Eds. Pratt, P. L.; et al., Chapman & Hall, London, 1969, p. 725. 2 Matsumoto, T.; Kitagawa, H., Int. Conf. on Mechanical Behavior of Materials, Jpn, 1971, Abstracts, V. 3A, Kyoto Int. Conf. Hall(KICH), August, 1971, Vol 1, p. 352. 3 Hahn, G. T.; Hoagland, R. G.; Rosentield, A. R., Metall. Trans., 3(1972) , 1189. 4 Pineau, A. G.; Pelloux, R. M., Metall. Trans., 5(1974) , 1103. 5 Bathias, C., Int. Conf. on Fracture, 4th Waterloo, 1977, Fracture 1977, V. 3A, Ed. Taplin, D. M. R., Pergamon, New York, 1978, Vol. 2, p. 1307. 6 Rice, J. R., Am. Soc. Test. Mater., Spec. Tech. Publ., 415, (1966) , p. 247. 7 Clavel, M.; Fournier, D.; Pineau, A., Metall. Trans., 6(1975) , 2305. 8 Lino, Y., Met. Sci., 10 (1976) , №. 5, 159. 9 Forsyth, P. J. E., Crack Propagation Symposium, Cranfield 1961, Proc. of the Crack Propagation Symp., Cranfield, Sept., 1961, Cranfield, the College of Aeronautics, 1962, p. 76. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|