| 不同玻璃态PdTa_1Si_(16.5)合金的热稳定性研究 |
| 宁远涛;郑云 |
| 冶金工业部贵金属研究所;冶金工业部贵金属研究所 |
|
| THE THERMAL STABILITY OF PdTa_1 Si_(16.5) ALLOY OF DIFFERENT GLASSY STATES |
| by NING Yuantao; ZHENG Yun(Institute of Precious Metals; Ministry of Metallurgical Industry; Kunming)(Manuscript received 26 April; 1983; revised manuscript 27 July; 1983) |
引用本文:
宁远涛;郑云. 不同玻璃态PdTa_1Si_(16.5)合金的热稳定性研究[J]. 金属学报, 1984, 20(2): 154-158.
,
.
THE THERMAL STABILITY OF PdTa_1 Si_(16.5) ALLOY OF DIFFERENT GLASSY STATES[J]. Acta Metall Sin, 1984, 20(2): 154-158.
1 Gao Yi-Qun(高逸群); Zheng Fu-Qian(关福前); Liu Xiong(刘雄);Ning Yuan-Tao(宁远涛), Proc. 4th Int. Conf. on Rapidly Quenched Metals(Sendai, 1981) , Eds. Masumoto, T.; Suzuki, K., JIM, 1982, Vol. 1, p. 727. 2 Chen, H. S., Appl. Phys. Lett., 29(1976) , 12. 3 Chen, H. S., Rep. Prog. Phys., 43(1980) , 353. 4 Freed, R. L.; Vander Sande, J. B., Acta Metall., 28(1980) , 103. |
|