| 液相淬火二元非晶态合金形成条件的实验探讨 |
| 刘志毅 |
| 中国科学院物理研究所 |
|
| EXPERIMENTAL STUDY OF CONDITION FOR BINARY AMORPHOUS ALLOYS FORMATION BY LIQUID QUENCHING |
| LIU Zhiyi(Institute of Physics; Academia Sinica; Beijing)(Manuscript received 2 August; 1982; revised manuscript 19 November; 1982) |
引用本文:
刘志毅. 液相淬火二元非晶态合金形成条件的实验探讨[J]. 金属学报, 1984, 20(1): 78-86.
.
EXPERIMENTAL STUDY OF CONDITION FOR BINARY AMORPHOUS ALLOYS FORMATION BY LIQUID QUENCHING[J]. Acta Metall Sin, 1984, 20(1): 78-86.
1 Takayama, S., J. Mater. Sci., 11 (1976) , 164. 2 Gissen, B.C.; Wager, C. N. J., Physics and Chemsitry of Liquid Metals, Ed. Beer, S. Z., Marcel Dekker, New York, 1972, p. 633. 3 Davies, H.A.; Aucote, J.; Hull, J.B., Scr. Metall., 8 (1974) , 1179. 4 Chen, H.S., Acta Metall., 22 (1974) , 1505. 5 Fujime, S., Jpn. J. Appl. Phys., 6 (1976) , 305. 6 Alder, B.J., J. Chem. Phys., 40 (1964) , 2724. 7 Adam, G.; Gibbs, J.H., ibid., 43 (1965) , 139. 8 Donald, L W.; Davies, H.A., J. Non-Cryst. Solids, 30 (1978) , 77. 9 Cohen, H, M.; Turnbull, D., Nature, 189 (1961) , 131. 10 Mader, S.; Nowick, A.S.; Widmer, H., Acta Metall., 15 (1967) , 203. 11 施天生;郑如龙;陈念贻,金属学报,15(1979) ,94. 12 宁远涛;周新铭,金属学报,17(1981) ,278. 13 张邦维,金属学报,17(1981) ,285. 14 Hansen, M.; Anderko, K., Constitution of Binary Alloys, McGraw-Hill, New York, 1958, p. 28, 212, 592. 15 Graebner, J.E.; Golding, B.; Schultz, R.J.; Hsu, F. S. L.; Chen, H. S., Phys. Rev. Lett., 39 (1977) , 1480. 16 Liu Zhi-yi (刘志毅); Jin Duo (金铎); Jin Zup-wen (金作文; Ma Ming-rong (马明荣); Zhao Zhong-xian (赵忠贤); Luo Qi-guang (罗启光), Chin. Phys., 2 (1982) , 486. 17 Liu Zhi-yi (刘志毅); Wang Chao-guo (王朝果); Cheng Peng-zhu (程鹏煮); Yang Da-yu (杨大宇); Ma Xiao-hua (马小华); Luo Qi-quang (罗启光), Chin. Phys., 2 (1982) , 489. 18 #12 19 Moffatt's Binary Phase Digram Handbook, General Electric Co., 1976. 20 刘志毅;王守证,低温物理,3(1981) ,235. 21 刘志毅;毕文;刘振兴,低温物理,2(1980) ,144 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|