| 淬火温度对4330M钢应力腐蚀的影响——晶界上杂质偏聚对高强度钢应力腐蚀开裂的作用 |
| 林栋梁;吴建生 |
| 上海交通大学;上海交通大学 |
|
| INFLUENCE OF QUENCHING TEMPERATURE ON STRESS CORROSION IN 4330M STEEL——The Role of Impurity Segregation in Stress Corrosion Cracking of High Strength Steel |
| LIN Dongliang (T. L. Lin); WU Jiansheng (Shanghai Jiaotong University) (Manuscript received 7 August; 1982) |
引用本文:
林栋梁;吴建生. 淬火温度对4330M钢应力腐蚀的影响——晶界上杂质偏聚对高强度钢应力腐蚀开裂的作用[J]. 金属学报, 1984, 20(1): 62-152.
,
.
INFLUENCE OF QUENCHING TEMPERATURE ON STRESS CORROSION IN 4330M STEEL——The Role of Impurity Segregation in Stress Corrosion Cracking of High Strength Steel[J]. Acta Metall Sin, 1984, 20(1): 62-152.
1 Zackay, V.E.; Parker, E.R.; Goolsby, R.D.; Wood, W.E., Nature Phys. Sci., 236(1972) , 108. 2 Lai, G.Y.; Wood, W.E.; Clark, R.A.; Zackay, V.F.; Parker, E. R., Metall. Trans., 5 (1974) , 1633. 3 Clark, G.; Ritchie, R.O.; Knott, J.F., Nature Phys. Sci., 239 (1972) , 104. 4 Richie, R.O.; Knott, J.F., Metall. Trans., 5 (1974) , 782. 5 褚武扬;李世琼;肖纪美;王枨,金属学报,16(1980) ,179. 6 McLean, D.; Grain Boundaries in Metals, Oxford Univ. Press, 1957. 7 Beachem, C.D., Metall. Trans., 3(1972) , 427. 8 小倉次夫;牧野彰宏;增本健,日本金属学会誌,45(1981) ,1093. 9 Thompson, A.W.; Bernstein, I.M., Stress Corrosion Cracking, Eds. Yahalom, J.; Aiqdjem, A. Freund Publ. House, 1980. p. 193. 10 Naylor, J.P.; Blondeau, R., Metall. Trans., 7A (1976) , 891. 11 Ucisik, A.H.; McMahon, C.J., Jr.; Feng, H, C., Metall. Trans., 9A (1978) , 321. 12 Lea, C., Met. Sci., 14 (1980) , 107. 13 Hondros, E.D., Proc. R. Soc., London, A286 (1965) , 479. 14 Troiano, A.R., Trans. ASM, 52(1960) , 54. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|