| C-Mn结构钢拉伸变形过程中空穴形核的研究——结构钢韧性断裂机理研究之一 |
| 史耀武;J.T.Barnby |
| 西安交通大学;英国阿斯顿大学 |
|
| VOID NUCLEATION IN TENSILE DEFORMATION PROCESSES OF C-Mn STRUCTURAL STEEL——Ductile Fracture Mechanisms in a Structural Steel (Ⅰ) |
| SHI Yaowu (Xi'an Jiaotong University); BARNBY J.T. (University of Aston; Birmingham; U.K.) (Manuscript received 21 March; 1983) |
引用本文:
史耀武;J.T.Barnby. C-Mn结构钢拉伸变形过程中空穴形核的研究——结构钢韧性断裂机理研究之一[J]. 金属学报, 1984, 20(1): 17-142.
,
.
VOID NUCLEATION IN TENSILE DEFORMATION PROCESSES OF C-Mn STRUCTURAL STEEL——Ductile Fracture Mechanisms in a Structural Steel (Ⅰ)[J]. Acta Metall Sin, 1984, 20(1): 17-142.
| 1 Rogers, H.C., Trans. Metall. Soc. AIME, 218 (1960) , 498.
2 Failure Analysis and Prevention, Metals Handbook, 8th ed., ASM, Vol. 10, Ohio, 1975, p. 61.
3 Shockey, D.A.; Seaman, L.; Dao, K.C.; Curran, R., A Computational Model for Fracture of Pressure Vessel Steel Derived from Experimental Data, Paper № 78-PVP-92, Presented at the ASME/CSME Pressure Vessels and Piping Conference, Montreal, Canada, June 1978.
4 Beremin, F.M., Metall. Trans., 12A(1981) , 723.
5 Fisher, J.R.; Gurland, J., Met. Sci., 15 (1981) , 185.
6 Barnby, J.T., Acta Metall., 15 (1967) , 903.
7 Tomota, Y.; Kawamura, Y.; Kuroki, K., Bull. JSME, 24 (1981) , 282.
8 Curry, D.A.; Pratt, P.L., Mater. Sci. Eng., 37 (1979) , 223.
9 Barnby, J.T.; Johnson, M.R., Met. Sci. J., 3 (1969) , 155.
10 Goods, S. H.; Brown, L.M., Acta Metall., 27 (1979) , 1.
11 Hancock, J.W.; Mackenzie, A.C., J. Mech. Phys. Solids, 24 (1976) , 147.
12 Shockey, D.A.; Dao, K.C.; Seaman, L.; Burback, R.; Curran, D.R., Computational Modelling of Microstructural Fracture Processes in A533B Pressure Vessel Steel, NP-1398, Research Project 1023-1, Final Report, Electric Power Research Institute, Palo Alto, California, May 1980.
13 Melander, A., Acta Metall, 28(1980) , 1799.
14 Shi Yao-wu, PhD Thesis, the University of Aston in Birmingham, 1982.
15 Edelson, B.I.; Baldwin, W.M., Jr., ASM Trans. Q., 55(1962) , 230.
16 LeRey, G.; Embury, J.D.; Edward, G.; Ashby, M.F., Acta Metall., 29 (1981) , 1509. |
|